What Is Inconel?

Inconel is a family of austenitic nickel-chromium-based superalloys or special steel. Inconel alloys are oxidation-corrosion-resistant materials well suited for service in extreme environments subjected to pressure and heat. When heated, Inconel forms a thick, stable, passivating oxide layer protecting the surface from further attack. Inconel Heat Resistance performance characteristics such as tensile strength, impact resistance, and corrosion resistance can degrade when the metal has been heated to a high temperature.


Inconel Material Specification

  • Inconel 600
    Solid solution strengthened.
  • Inconel 601
  • Inconel 625
    Acid resistant, good weldability. The LCF version is typically used in bellows. Ideal for hardware and components in the power, aerospace and chemical processing industries. Offered in sheet, plate, bar and forgings.
  • Inconel 718
    Gamma double prime strengthened with good weldability. The preferred material for cryogenic storage tanks, turbines, downhole shafts and wellhead parts offered in sheet, plate and bar.

Inconel density & Inconel Properties

Inconel Tensile Strength

  Physical Properties Metric English
Inconel Alloy 600 Density 8.47 g/cc 0.306 lb/in³
Inconel Alloy 625 Density 8.44 g/cc 0.305 lb/in³
Inconel Alloy 718 Density 8.19 0.296 lb/in3 (8.192 g/cm3)

Inconel Alloy 625 Density*. 8440 [kg · m-3
Inconel Alloy 625 Density: 0.303 lb/in3 (8.44 g/cm3)


Inconel Electrical Conductivity

Material Conductivity Resistivity Notes
(% IACS) (Siemens/m) (Ohm-m)  

Inconel 600

1.70

9.860E+05

1.014E-06

conductivity converted from resistivity

Inconel 600

1.67

1.030E-06

conductivity converted from resistivity

Inconel 601

1.45

1.190E-06

conductivity converted from resistivity

Inconel 617

1.41

1.220E-06

conductivity converted from resistivity

Inconel 625

1.34

1.290E-06

conductivity converted from resistivity

Inconel 690

11.65

1.480E-07

conductivity converted from resistivity

Inconel 718

1.38

1.250E-06

conductivity converted from resistivity

Inconel X750

1.41

1.220E-06

conductivity converted from resistivity

Inconel Hardness

Inconel Rockwell Hardness, Inconel Strength

Material Hardness HB
Inconel Alloy 625 Bar
≤ 287 HB
Inconel Alloy 625 Sheet
145-240
Inconel Alloy 625 Tube
Seamless and Welded
-
Inconel Alloy 600 rod and bar
65-85B
Inconel Alloy 600 Plate
65-85B
Inconel Alloy 600 Sheet
88B max
Inconel Alloy 600 Tube and Pipe
88B max
Inconel Alloy 600 Wire
-
Inconel Alloy 600 Wire
-
Inconel Alloy 600 Wire
-

Inconel Heat Treatment

Heat Treatment Inconel Alloy 600 Inconel Alloy 600 is not an age hardening alloy; cold working is the only available means of hardening. Softening by annealing begins at about 1600°F (871°C), and is reasonably complete after 10 to 15 minutes of heating at 1800°F (982°C). Above this temperature, grain growth may be objectionable, although very brief heating at 1900°F will cause complete softening without undue grain growth. Since the rate of cooling has no effect on the softening, the material may be water quenched or air cooled.
Heat Treatment Inconel Alloy 625 Inconel Alloy 625 has three basic heat treatments:
(1) High Solution Anneal - 2000/2200°F (1093/1204°C), air quench or faster.
(2) Low Solution Anneal - 1700/1900°F (927/1038°C), air quench or faster.
(3) Stress Relieve - 1650°F (899°C), air quench.
Inconel Heat Shield Inconel (2200 deg F continuous).

Inconel Low Temperature

Inconel Alloy 718 temperature ranges from cryogenic up to 1400°F
Inconel Alloy 625 temperatures ranging from cryogenic to 2000°F

Inconel Melting Point

Inconel Alloy 718 Melting Range Solution Treated: 2500-2600°F
Solution Treated and Aged: 1370-1430°C
Inconel Alloy 600 Melting Range Metric: 1354 - 1413 °C
English: 2470 - 2580 °F
Inconel Alloy 625 Melting Range 2350 - 2460°F (1280 - 1350°C)

Inconel Thermal Conductivity

Inconel Thermal Properties, Inconel Thermal Expansion

Inconel Alloy 600 Thermal Conductivity

Metric: 14.9 W/m-K
English: 103 BTU-in/hr-ft²-°F

Inconel Alloy 625 Thermal Conductivity Metric: 9.8 W/m-K
English: 68 BTU-in/hr-ft²-°F

Inconel Temperature Limits

Inconel Alloy 600 Heat Capacity

Metric: 0.444 J/g-°C
English: 0.106 BTU/lb-°F

Inconel Alloy 625 Heat Capacity Metric: 0.41 J/g-°C
English: 0.098 BTU/lb-°F

Inconel Mechanical Properties

Typical Mechanical Properties

Inconel Machinability and Inconel Yield Strength

Material Form and Condition Tensile Strength Yield Strength Elongation % Hardness, Rockwell
ksi MPa ksi MPa
Inconel Alloy 600 rod and bar Cold drawn Annealed 80-100 550-690 25-50 170-345 55-35 65-85B
Inconel Alloy 600 Plate Hot rolled Annealed 80-100 550-725 30-50 205-345 55-35 65-85B
Inconel Alloy 600 Sheet Cold Rolled Annealed 80-100 550-690 30-45 205-310 55-35 88B max
Inconel Alloy 600 Tube and Pipe Cold Drawn Annealed 80-100 550-690 25-50 170-345 55-35 88B max
Inconel Alloy 600 Wire Cold Drawn Annealed 80-120 550-830 35-75 240-520 45-20 -
Inconel Alloy 600 Wire Cold Drawn No 1 Temper 105-135 725-930 70-105 480-725 35-15 -
Inconel Alloy 600 Wire Spring Temper 170-220 1170-1520 150-210 1035-1450 5-2 -
Inconel Alloy 625 Bar Annealed 120 827 60 414 30 ≤ 287 HB
Inconel Alloy 625 Sheet Annealed 120 827 60 414 30 145-240
Inconel Alloy 625 Tube
Seamless and Welded
Annealed 120 827 60 414 35 -

 