SPECIALIZED IN TITANIUM & NICKEL ALLOYS
SHEET / PLATE, TUBES, PIPES, WIRES, ROUND BARS, WELDING CONSUMABLES

Hastelloy C22 Supplier

Hastelloy C22 price in India, Hastelloy C22 material stockist in India, Hastelloy C22 Products suppliers, Hastelloy C22 material distributor in India, Hastelloy C22 material dealers in Mumbai, India



Hastelloy C22 Suppliers in India

 

What Is Hastelloy C22?

Hastelloy C22, also known as alloy C22, is a versatile austenitic nickel-chromium-molybdenum-tungsten alloy with enhanced resistance to pitting, crevice corrosion and stress corrosion cracking. The high chromium content provides good resistance to oxidizing media while the molybdenum and tungsten content give good resistance to reducing media. Hastelloy C-22 has resistance to are oxidizing acid chlorides, wet chlorine, formic and acetic acids, ferric and cupric chlorides, sea water, brine and many mixed or contaminated chemical solutions, both organic and inorganic.


HASTELLOY® C-22

UNS Number N06022

Other common names: Alloy C22

In what forms is Hastelloy C22 Available at Aries Alloys?

  • Sheet
  • Plate
  • Bar
  • Pipe & Tube (welded & seamless)
  • Fittings (i.e. flanges, slip-ons, blinds, weld-necks, lapjoints, long welding necks, socket welds, elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples)
  • Wire
Hastelloy C22 Chemical Composition
C Cr Co Fe Mn Mo Ni P
.010 max 20-22.5 2.5 max 2.0-6.0 .50 max 12.5-14.5 Balance .02 max
Si S W V        
.08 max .02 max 2.5-3.5 .35 max        

ASTM Specifications

Pipe Smls
Pipe Welded
Tube Smls
Tube Welded
Sheet/Plate
Bar
Forging
Fitting
B622
B619 B622 B626 B575 B574 B564 B366

Mechanical Properties
Typical Room Temperature Tensile Properties of Annealed Material

Product Form Tensile (ksi) .2% Yield (ksi) Elongation % Hardness (HRb)
Plate (.25”-1.75”) 112 53 62 89
Sheet (.038”-.15”) 122 63 54 93
Bar (.50”-5.50”) 115 55 60 89

Hastelloy C22 Melting Point

Physical Properties

°F

British Units

°C

Metric Units

Density

75

0.314 lb./in.(3)

24

8.69 g/cm(3)

Melting Range

2475-
2550

1357-
1399

Electrical
Resistivity

75

44.8 microhm-in.

24

1.14 microhm-m

212

48.3 microhm-in.

100

1.23 microhm-m

392

48.7 microhm-in.

200

1.24 microhm-m

572

49.3 microhm-in.

300

1.25 microhm-m

752

49.6 microhm-in.

400

1.26 microhm-m

932

49.9 microhm-in.

500

1.27 microhm-m

1112

50.2 microhm-in.

600

1.28 microhm-m

Mean Coefficient
of Thermal
Expansion

75-200

6.9 microin./in.-°F

24-93

12.4 X 10(-6)m/m-K

75-400

6.9 microin./in.-°F

24-204

12.4 X 10(-6)m/m-K

75-600

7.0 microin./in.-°F

24-316

12.6 X 10(-6)m/m-K

75-800

7.4 microin./in.-°F

24-427

13.3 X 10(-6)m/m-K

75-1000

7.7 microin./in.-°F

24-538

13.9 X 10(-6)m/m-K

75-1200

8.1 microin./in.-°F

24-649

14.6 X 10(-6)m/m-K

75-1400

8.5 microin./in.-°F

24-760

15.3 X 10(-6)m/m-K

75-1600

8.8 microin./in.-°F

24-871

15.8 X 10(-6)m/m-K

75-1800

9.0 microin./in.-°F

24-982

16.2 X 10(-6)m/m-K

Thermal
Conductivity

118

70 Btu-in/ft²-hr-°F

48

10.1 W/m-K

212

77 Btu-in/ft²-hr-°F

100

11.1 W/m-K

392

93 Btu-in/ft²-hr-°F

200

13.4 W/m-K

572

108 Btu-in/ft²-hr-°F

300

15.5 W/m-K

752

121 Btu-in/ft²-hr-°F

400

17.5 W/m-K

932

135 Btu-in/ft²-hr-°F

500

19.5 W/m-K

1112

148 Btu-in/ft²-hr-°F

600

21.3 W/m-K

Thermal
Diffusivity

70

0.004 in²/sec

21

2.7 x 10(-6)m²/s

212

0.005 in²/sec

100

3.0 x 10(-6)m²/s

392

0.005 in²/sec

200

3.5 x 10(-6)m²/s

572

0.006 in²/sec

300

3.9 x 10(-6)m²/s

752

0.007 in²/sec

400

4.2 x 10(-6)m²/s

932

0.007 in²/sec

500

4.6 x 10(-6)m²/s

1112

0.007 in²/sec

600

4.8 x 10(-6)m²/s


Hastelloy C22 Price per Pound

Hastelloy C22 Price in India: US $10-12 per Pound

 

 


Return to top