Hastelloy C22 Supplier
Hastelloy C22 price in India, Hastelloy C22 material stockist in India, Hastelloy C22 Products suppliers, Hastelloy C22 material distributor in India, Hastelloy C22 material dealers in Mumbai, India
Table Of Content:
Hastelloy C22 Suppliers in India
What Is Hastelloy C22?
Hastelloy C22, also known as alloy C22, is a versatile austenitic nickel-chromium-molybdenum-tungsten alloy with enhanced resistance to pitting, crevice corrosion and stress corrosion cracking. The high chromium content provides good resistance to oxidizing media while the molybdenum and tungsten content give good resistance to reducing media. Hastelloy C-22 has resistance to are oxidizing acid chlorides, wet chlorine, formic and acetic acids, ferric and cupric chlorides, sea water, brine and many mixed or contaminated chemical solutions, both organic and inorganic.
HASTELLOY® C-22
UNS Number N06022
Other common names: Alloy C22
In what forms is Hastelloy C22 Available at Aries Alloys?
- Sheet
- Plate
- Bar
- Pipe & Tube (welded & seamless)
- Fittings (i.e. flanges, slip-ons, blinds, weld-necks, lapjoints, long welding necks, socket welds, elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples)
- Wire
Hastelloy C22 Chemical Composition
C | Cr | Co | Fe | Mn | Mo | Ni | P |
---|---|---|---|---|---|---|---|
.010 max | 20-22.5 | 2.5 max | 2.0-6.0 | .50 max | 12.5-14.5 | Balance | .02 max |
Si | S | W | V | ||||
.08 max | .02 max | 2.5-3.5 | .35 max |
ASTM Specifications
Pipe Smls |
Pipe Welded |
Tube Smls |
Tube Welded |
Sheet/Plate |
Bar |
Forging |
Fitting |
---|---|---|---|---|---|---|---|
B622 |
B619 | B622 | B626 | B575 | B574 | B564 | B366 |
Mechanical Properties
Typical Room Temperature Tensile Properties of Annealed Material
Product Form | Tensile (ksi) | .2% Yield (ksi) | Elongation % | Hardness (HRb) |
---|---|---|---|---|
Plate (.25”-1.75”) | 112 | 53 | 62 | 89 |
Sheet (.038”-.15”) | 122 | 63 | 54 | 93 |
Bar (.50”-5.50”) | 115 | 55 | 60 | 89 |
Hastelloy C22 Melting Point
Physical Properties |
°F |
British Units |
°C |
Metric Units |
Density |
75 |
0.314 lb./in.(3) |
24 |
8.69 g/cm(3) |
Melting Range |
2475- |
1357- |
||
Electrical |
75 |
44.8 microhm-in. |
24 |
1.14 microhm-m |
212 |
48.3 microhm-in. |
100 |
1.23 microhm-m |
|
392 |
48.7 microhm-in. |
200 |
1.24 microhm-m |
|
572 |
49.3 microhm-in. |
300 |
1.25 microhm-m |
|
752 |
49.6 microhm-in. |
400 |
1.26 microhm-m |
|
932 |
49.9 microhm-in. |
500 |
1.27 microhm-m |
|
1112 |
50.2 microhm-in. |
600 |
1.28 microhm-m |
|
Mean Coefficient |
75-200 |
6.9 microin./in.-°F |
24-93 |
12.4 X 10(-6)m/m-K |
75-400 |
6.9 microin./in.-°F |
24-204 |
12.4 X 10(-6)m/m-K |
|
75-600 |
7.0 microin./in.-°F |
24-316 |
12.6 X 10(-6)m/m-K |
|
75-800 |
7.4 microin./in.-°F |
24-427 |
13.3 X 10(-6)m/m-K |
|
75-1000 |
7.7 microin./in.-°F |
24-538 |
13.9 X 10(-6)m/m-K |
|
75-1200 |
8.1 microin./in.-°F |
24-649 |
14.6 X 10(-6)m/m-K |
|
75-1400 |
8.5 microin./in.-°F |
24-760 |
15.3 X 10(-6)m/m-K |
|
75-1600 |
8.8 microin./in.-°F |
24-871 |
15.8 X 10(-6)m/m-K |
|
75-1800 |
9.0 microin./in.-°F |
24-982 |
16.2 X 10(-6)m/m-K |
|
Thermal |
118 |
70 Btu-in/ft²-hr-°F |
48 |
10.1 W/m-K |
212 |
77 Btu-in/ft²-hr-°F |
100 |
11.1 W/m-K |
|
392 |
93 Btu-in/ft²-hr-°F |
200 |
13.4 W/m-K |
|
572 |
108 Btu-in/ft²-hr-°F |
300 |
15.5 W/m-K |
|
752 |
121 Btu-in/ft²-hr-°F |
400 |
17.5 W/m-K |
|
932 |
135 Btu-in/ft²-hr-°F |
500 |
19.5 W/m-K |
|
1112 |
148 Btu-in/ft²-hr-°F |
600 |
21.3 W/m-K |
|
Thermal |
70 |
0.004 in²/sec |
21 |
2.7 x 10(-6)m²/s |
212 |
0.005 in²/sec |
100 |
3.0 x 10(-6)m²/s |
|
392 |
0.005 in²/sec |
200 |
3.5 x 10(-6)m²/s |
|
572 |
0.006 in²/sec |
300 |
3.9 x 10(-6)m²/s |
|
752 |
0.007 in²/sec |
400 |
4.2 x 10(-6)m²/s |
|
932 |
0.007 in²/sec |
500 |
4.6 x 10(-6)m²/s |
|
1112 |
0.007 in²/sec |
600 |
4.8 x 10(-6)m²/s |
Hastelloy C22 Price per Pound
Hastelloy C22 Price in India: US $10-12 per Pound